Tensile strength warp / weft
| 750 N per 5 cm
|
Tear strength warp / weft
| 200 N
|
FR performance
| EN 13501-1 class B
|
|
|
|
Tensile strength warp / weft
| 1000 N per 5 cm
|
Tear strength warp / weft
| 210 N
|
UV stability
| 300 Kly
|
FR performance
| EN 13501-1 class B
|
|
|
|
Tensile strength warp / weft
| 1800 N per 5 cm
|
UV stability
| 300 Kly
|
|
|
|
Tensile strength warp / weft
| 620 N per 5 cm
|
Tear strength warp / weft
| 168 N
|
|
|
|
Tensile strength warp / weft
| 610 N per 5 cm
|
Tear strength warp / weft
| 165 N
|
UV stability
| 300 Kly
|
|
|
|
Tensile strength warp / weft
| 800 / 750 N per 5 cm
|
Tear strength warp / weft
| 190 / 200 N
|
UV stability
| 300 Kly
|
|
|
|
|
|
|
|